Kodak Tri-X Pan Film | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Packaged Developers 65° F | 18.5° C 68° F | 20° C 70° F | 21° C 72° F | 22° C 74° F | 24° C HC-110 | 8½ | 7½ | 6½ | 6 | 5 | Polydol | 8 | 7 | 6½ | 6 | 5 | D-76 | 9 | 8 | 7½ | 6½ | 5½ | D-76 (1:1) | 11 | 10 | 9½ | 9 | 8 | Microdol-X | 11 | 10 | 9½ | 9 | 8 | Microdol-X (1:3) | --- | --- | 15 | 14 | 13 | DK-50 (1:1) | 7 | 6 | 5½ | 5 | 4½ | HC-110 | 4½ | 3¾ | 3¼ | 3 | 2½ | *Avoid development times of less than 5 minutes if possible, because poor uniformity may result. | Note: Do not use developers containing silver halide solvents. | |||||||||||||||